PVC Pipe Parallel Screw Barrel
  • PVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw Barrel

PVC Pipe Parallel Screw Barrel

Nanhaiya's custom-designed PVC Pipe Parallel Screw Barrel yakagadzirwa nepamusoro-magumo 38CrMoAlA nitrided simbi, zvichiita kuti iwedzere kupfeka kuramba, kusaita ngura, uye simba. Iyi screw barrel assembly ndiyo yakakosha vimbiso yekushanda uye yakagadzikana PVC pombi extrusion. Kana iwe uchitsvaga yepamusoro-inoshanda imwe screw solution, ndapota taura nesu kuti uwane ruzivo rwakadzama rwehunyanzvi uye quote.

Yedu PVC Pipe Parallel Screw Barrel yakagadzirwa nepamusoro-kuita extrusion yePVC pombi zvigadzirwa, kuve nechokwadi chepurasitiki chakanakisa, kubuda kwepamusoro, uye hupenyu hurefu hwesevhisi. Yakagadzirirwa kusangana nezvinodiwa zvePVC komputa, isu tinopa yakazara maitiro mujometry uye simbi kuti iwedzere kupfeka uye kusagadzikana kwekuora.

Chigadzirwa Parameter (Kutsanangurwa)

Material

38CrMoAlA

Kupisa Kurapa Kuoma

HB260-320

Nitriding Hardness

HV950-1000

Nitriding Depth

0.50-0.70mm

Nitriding Brittleness

≤giredhi 1

Kukasharara

Ra0.4

Kururama kweScrew

0.015mm

Chrome Plating Kuoma

HV≥950HV

Chrome Kukora

0.05-0.10mm

Bimetal Hardness

HRC60-65

Bimetal Depth

2.0-3.0mm

Product Feature uye Application

Yedu PVC Pipe Parallel Screw Barrel yakagadzirirwa kushanda uye yakagadzikana yakasimba PVC extrusion. Iine optimized screw geometry uye yakasimba alloy zvinhu, inovimbisa yakanakisa plasticizing, yakatsetseka pamusoro pekupedzisira, uye yakakwirira kubuda kuita. Inoratidzira kupfeka kwepamusoro uye kusagadzikana kwekuora, hupenyu hurefu hwesevhisi, uye sarudzo dzakazara dzekugadzirisa, inoshandiswa zvakanyanya mukugadzira pombi dzemvura nemadhiraini, mapombi emagetsi, pombi dzekudzivirira, uye mamwe ekuvaka-giredhi PVC pombi masisitimu.

PVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw Barrel

Product Details

• Material Options: 38CrMoAlA nitrided simbi, bimetallic alloy, high-speed simbi, HIP hupfu simbi

• Kuoma Kwepamusoro: Nitriding kuoma HV ≥ 900; kupfeka kwakasimba uye kusagadzikana kwekuora

• Diameter Range: Φ45 mm - Φ150 mm (inogoneka)

• L/D Ratio: 32–38 kana kuti yakanangana nezvinodiwa zvekugadzira

• Processing Technology: Precision CNC machining, nitriding kurapwa, polishing, alloy coating iripo

• Kugarisana: Inokodzera mhando huru dzeextruder (KraussMaffei, Cincinnati, Jwell, nezvimwewo)

• Structure Design: Customized sikuruu profile, compression reshiyo, venting dhizaini, kudziyisa nzvimbo

• Kuvimbiswa Kwehutano: Kudzora kwakasimba kushivirira uye kusimba kwekuenzanisa kwekuenzanisa kuti ive nechokwadi che extrusion yakagadzikana

PVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw BarrelPVC Pipe Parallel Screw Barrel
Sravana Sameeralu Serial 4th Hot Tags: PVC Pipe Parallel Screw Barrel, Mugadziri, Mutengesi, Factory
Send Inquiry
Contact Info
Kugamuchirwa kune webhusaiti yedu! Zvekubvunza nezve zvigadzirwa zvedu kana pricelist, ndapota siya email yako kwatiri uye isu tichabatana mukati memaawa makumi maviri nemana.
X
Isu tinoshandisa makuki kukupa iwe zvirinani kubhurawuza ruzivo, kuongorora saiti traffic uye kugadzirisa zvemukati. Nekushandisa saiti ino, unobvuma kushandisa kwedu makuki.Privacy Policy
RambaGamuchira